{"id":423,"date":"2026-04-04T17:39:48","date_gmt":"2026-04-04T17:39:48","guid":{"rendered":"https:\/\/ifo.le-an.net\/?post_type=dienstleistung&#038;p=423"},"modified":"2026-04-04T17:39:49","modified_gmt":"2026-04-04T17:39:49","slug":"mono-impact-test","status":"publish","type":"dienstleistung","link":"https:\/\/ifo.le-an.net\/en\/dienstleistungen\/monoschlagpruefung\/","title":{"rendered":"Mono impact test"},"content":{"rendered":"<p>In the mono impact test, a hardened steel ball with a diameter of 5 mm is fired at the surface to be tested with a defined force (up to 90 N). The coating is then tested for cracks or flaking.<\/p>","protected":false},"excerpt":{"rendered":"<p>In the mono impact test, a hardened steel ball with a diameter of 5 mm is fired at the surface to be tested with a defined force (up to 90 N). The coating is then tested for cracks or flaking.<\/p>","protected":false},"featured_media":419,"template":"","meta":{"_acf_changed":true},"class_list":["post-423","dienstleistung","type-dienstleistung","status-publish","has-post-thumbnail","hentry"],"acf":[],"_links":{"self":[{"href":"https:\/\/ifo.le-an.net\/en\/wp-json\/wp\/v2\/dienstleistung\/423","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/ifo.le-an.net\/en\/wp-json\/wp\/v2\/dienstleistung"}],"about":[{"href":"https:\/\/ifo.le-an.net\/en\/wp-json\/wp\/v2\/types\/dienstleistung"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/ifo.le-an.net\/en\/wp-json\/wp\/v2\/media\/419"}],"wp:attachment":[{"href":"https:\/\/ifo.le-an.net\/en\/wp-json\/wp\/v2\/media?parent=423"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}